How to dry out epoxy resin faster than usual?
I made MDF coasters and decorated them using epoxy resin with attractive colors and pearl powder.
It took 25-30 hours to completely dry out. In the meantime, few dust particles settled on it and I lost its glow.
How to dry it out faster?
Or better, how should I avoid this the next time?
material-selection preparation epoxy-resin
New contributor
add a comment |
I made MDF coasters and decorated them using epoxy resin with attractive colors and pearl powder.
It took 25-30 hours to completely dry out. In the meantime, few dust particles settled on it and I lost its glow.
How to dry it out faster?
Or better, how should I avoid this the next time?
material-selection preparation epoxy-resin
New contributor
BTW, a weird thing about English is that "few" and "a few" kinda mean opposite things.
– Acccumulation
Apr 19 at 14:48
add a comment |
I made MDF coasters and decorated them using epoxy resin with attractive colors and pearl powder.
It took 25-30 hours to completely dry out. In the meantime, few dust particles settled on it and I lost its glow.
How to dry it out faster?
Or better, how should I avoid this the next time?
material-selection preparation epoxy-resin
New contributor
I made MDF coasters and decorated them using epoxy resin with attractive colors and pearl powder.
It took 25-30 hours to completely dry out. In the meantime, few dust particles settled on it and I lost its glow.
How to dry it out faster?
Or better, how should I avoid this the next time?
material-selection preparation epoxy-resin
material-selection preparation epoxy-resin
New contributor
New contributor
edited Apr 19 at 10:45
Erica♦
2,80531148
2,80531148
New contributor
asked Apr 19 at 8:37
shripal mehtashripal mehta
337
337
New contributor
New contributor
BTW, a weird thing about English is that "few" and "a few" kinda mean opposite things.
– Acccumulation
Apr 19 at 14:48
add a comment |
BTW, a weird thing about English is that "few" and "a few" kinda mean opposite things.
– Acccumulation
Apr 19 at 14:48
BTW, a weird thing about English is that "few" and "a few" kinda mean opposite things.
– Acccumulation
Apr 19 at 14:48
BTW, a weird thing about English is that "few" and "a few" kinda mean opposite things.
– Acccumulation
Apr 19 at 14:48
add a comment |
2 Answers
2
active
oldest
votes
To cure them more quickly you can either:
- use heat lamps or an electric heater over your resin pieces
- raise the temperature of the room they are in to say, 75 - 85°F / 24 - 30°C.
If you do either of these, you must maintain the heat constantly until fully cured.
Don't be tempted to add more hardener as it can stop the resin curing and remain sticky indefinitely.
There are additives that promote curing (called accelerator) however they are typically yellow in colour so will add a slight yellow hue to the resin. Also, the faster the resin cures, the greater the chance of it yellowing as a combination of the heat by-product of resin curing and heat applied to cure the resin faster.
There are reduced accelerator resins around which are slower curing but cure clearer.
To prevent dust from settling on the resin while curing, you can cover them with a cloche or bowl.
For more info on what I have said, you can read what ArtResin say at https://www.artresin.com/blogs/artresin/44707073-how-to-make-resin-cure-faster
I live in that part of India where the Temp is 40+ ℃
– shripal mehta
Apr 19 at 11:11
add a comment |
Make sure that you mixed the resin components in proper proportions and for long enough to achieve a homogeneous blend. If the components are not mixed thoroughly, some of the resin will cure slowly or not at all.
Not including enough hardener will definitely increase the curing time. Check the instructions to see if the proportions are by weight or by volume. 50/50 by weight can be dramatically different than 50/50 by volume.
Unrelated to your question but worth noting... working with resin in warm environments creates additional challenges, specifically related to heat. Almost all resins will crack and deform while curing if their heat rises above the limits of the material. To avoid such issues, you need to apply the resin in thin layers and allow each to mostly cure before adding the next. I started a river table resin pour on a cold night and was able to safely apply four layers, each 1/2 inch thick. The next day, during a hot high noon, I added a fifth 1/2 inch layer and cracks appeared everywhere, penetrating down through the previous nights layers. The project was ruined and now hangs on my shop wall as a reminder to watch resin temperatures and apply resin thinly.
Thanks for the tips! 👍
– shripal mehta
Apr 20 at 4:57
add a comment |
Your Answer
StackExchange.ready(function() {
var channelOptions = {
tags: "".split(" "),
id: "650"
};
initTagRenderer("".split(" "), "".split(" "), channelOptions);
StackExchange.using("externalEditor", function() {
// Have to fire editor after snippets, if snippets enabled
if (StackExchange.settings.snippets.snippetsEnabled) {
StackExchange.using("snippets", function() {
createEditor();
});
}
else {
createEditor();
}
});
function createEditor() {
StackExchange.prepareEditor({
heartbeatType: 'answer',
autoActivateHeartbeat: false,
convertImagesToLinks: false,
noModals: true,
showLowRepImageUploadWarning: true,
reputationToPostImages: null,
bindNavPrevention: true,
postfix: "",
imageUploader: {
brandingHtml: "Powered by u003ca class="icon-imgur-white" href="https://imgur.com/"u003eu003c/au003e",
contentPolicyHtml: "User contributions licensed under u003ca href="https://creativecommons.org/licenses/by-sa/3.0/"u003ecc by-sa 3.0 with attribution requiredu003c/au003e u003ca href="https://stackoverflow.com/legal/content-policy"u003e(content policy)u003c/au003e",
allowUrls: true
},
noCode: true, onDemand: true,
discardSelector: ".discard-answer"
,immediatelyShowMarkdownHelp:true
});
}
});
shripal mehta is a new contributor. Be nice, and check out our Code of Conduct.
Sign up or log in
StackExchange.ready(function () {
StackExchange.helpers.onClickDraftSave('#login-link');
});
Sign up using Google
Sign up using Facebook
Sign up using Email and Password
Post as a guest
Required, but never shown
StackExchange.ready(
function () {
StackExchange.openid.initPostLogin('.new-post-login', 'https%3a%2f%2fcrafts.stackexchange.com%2fquestions%2f6117%2fhow-to-dry-out-epoxy-resin-faster-than-usual%23new-answer', 'question_page');
}
);
Post as a guest
Required, but never shown
2 Answers
2
active
oldest
votes
2 Answers
2
active
oldest
votes
active
oldest
votes
active
oldest
votes
To cure them more quickly you can either:
- use heat lamps or an electric heater over your resin pieces
- raise the temperature of the room they are in to say, 75 - 85°F / 24 - 30°C.
If you do either of these, you must maintain the heat constantly until fully cured.
Don't be tempted to add more hardener as it can stop the resin curing and remain sticky indefinitely.
There are additives that promote curing (called accelerator) however they are typically yellow in colour so will add a slight yellow hue to the resin. Also, the faster the resin cures, the greater the chance of it yellowing as a combination of the heat by-product of resin curing and heat applied to cure the resin faster.
There are reduced accelerator resins around which are slower curing but cure clearer.
To prevent dust from settling on the resin while curing, you can cover them with a cloche or bowl.
For more info on what I have said, you can read what ArtResin say at https://www.artresin.com/blogs/artresin/44707073-how-to-make-resin-cure-faster
I live in that part of India where the Temp is 40+ ℃
– shripal mehta
Apr 19 at 11:11
add a comment |
To cure them more quickly you can either:
- use heat lamps or an electric heater over your resin pieces
- raise the temperature of the room they are in to say, 75 - 85°F / 24 - 30°C.
If you do either of these, you must maintain the heat constantly until fully cured.
Don't be tempted to add more hardener as it can stop the resin curing and remain sticky indefinitely.
There are additives that promote curing (called accelerator) however they are typically yellow in colour so will add a slight yellow hue to the resin. Also, the faster the resin cures, the greater the chance of it yellowing as a combination of the heat by-product of resin curing and heat applied to cure the resin faster.
There are reduced accelerator resins around which are slower curing but cure clearer.
To prevent dust from settling on the resin while curing, you can cover them with a cloche or bowl.
For more info on what I have said, you can read what ArtResin say at https://www.artresin.com/blogs/artresin/44707073-how-to-make-resin-cure-faster
I live in that part of India where the Temp is 40+ ℃
– shripal mehta
Apr 19 at 11:11
add a comment |
To cure them more quickly you can either:
- use heat lamps or an electric heater over your resin pieces
- raise the temperature of the room they are in to say, 75 - 85°F / 24 - 30°C.
If you do either of these, you must maintain the heat constantly until fully cured.
Don't be tempted to add more hardener as it can stop the resin curing and remain sticky indefinitely.
There are additives that promote curing (called accelerator) however they are typically yellow in colour so will add a slight yellow hue to the resin. Also, the faster the resin cures, the greater the chance of it yellowing as a combination of the heat by-product of resin curing and heat applied to cure the resin faster.
There are reduced accelerator resins around which are slower curing but cure clearer.
To prevent dust from settling on the resin while curing, you can cover them with a cloche or bowl.
For more info on what I have said, you can read what ArtResin say at https://www.artresin.com/blogs/artresin/44707073-how-to-make-resin-cure-faster
To cure them more quickly you can either:
- use heat lamps or an electric heater over your resin pieces
- raise the temperature of the room they are in to say, 75 - 85°F / 24 - 30°C.
If you do either of these, you must maintain the heat constantly until fully cured.
Don't be tempted to add more hardener as it can stop the resin curing and remain sticky indefinitely.
There are additives that promote curing (called accelerator) however they are typically yellow in colour so will add a slight yellow hue to the resin. Also, the faster the resin cures, the greater the chance of it yellowing as a combination of the heat by-product of resin curing and heat applied to cure the resin faster.
There are reduced accelerator resins around which are slower curing but cure clearer.
To prevent dust from settling on the resin while curing, you can cover them with a cloche or bowl.
For more info on what I have said, you can read what ArtResin say at https://www.artresin.com/blogs/artresin/44707073-how-to-make-resin-cure-faster
answered Apr 19 at 10:12
Chris RogersChris Rogers
538210
538210
I live in that part of India where the Temp is 40+ ℃
– shripal mehta
Apr 19 at 11:11
add a comment |
I live in that part of India where the Temp is 40+ ℃
– shripal mehta
Apr 19 at 11:11
I live in that part of India where the Temp is 40+ ℃
– shripal mehta
Apr 19 at 11:11
I live in that part of India where the Temp is 40+ ℃
– shripal mehta
Apr 19 at 11:11
add a comment |
Make sure that you mixed the resin components in proper proportions and for long enough to achieve a homogeneous blend. If the components are not mixed thoroughly, some of the resin will cure slowly or not at all.
Not including enough hardener will definitely increase the curing time. Check the instructions to see if the proportions are by weight or by volume. 50/50 by weight can be dramatically different than 50/50 by volume.
Unrelated to your question but worth noting... working with resin in warm environments creates additional challenges, specifically related to heat. Almost all resins will crack and deform while curing if their heat rises above the limits of the material. To avoid such issues, you need to apply the resin in thin layers and allow each to mostly cure before adding the next. I started a river table resin pour on a cold night and was able to safely apply four layers, each 1/2 inch thick. The next day, during a hot high noon, I added a fifth 1/2 inch layer and cracks appeared everywhere, penetrating down through the previous nights layers. The project was ruined and now hangs on my shop wall as a reminder to watch resin temperatures and apply resin thinly.
Thanks for the tips! 👍
– shripal mehta
Apr 20 at 4:57
add a comment |
Make sure that you mixed the resin components in proper proportions and for long enough to achieve a homogeneous blend. If the components are not mixed thoroughly, some of the resin will cure slowly or not at all.
Not including enough hardener will definitely increase the curing time. Check the instructions to see if the proportions are by weight or by volume. 50/50 by weight can be dramatically different than 50/50 by volume.
Unrelated to your question but worth noting... working with resin in warm environments creates additional challenges, specifically related to heat. Almost all resins will crack and deform while curing if their heat rises above the limits of the material. To avoid such issues, you need to apply the resin in thin layers and allow each to mostly cure before adding the next. I started a river table resin pour on a cold night and was able to safely apply four layers, each 1/2 inch thick. The next day, during a hot high noon, I added a fifth 1/2 inch layer and cracks appeared everywhere, penetrating down through the previous nights layers. The project was ruined and now hangs on my shop wall as a reminder to watch resin temperatures and apply resin thinly.
Thanks for the tips! 👍
– shripal mehta
Apr 20 at 4:57
add a comment |
Make sure that you mixed the resin components in proper proportions and for long enough to achieve a homogeneous blend. If the components are not mixed thoroughly, some of the resin will cure slowly or not at all.
Not including enough hardener will definitely increase the curing time. Check the instructions to see if the proportions are by weight or by volume. 50/50 by weight can be dramatically different than 50/50 by volume.
Unrelated to your question but worth noting... working with resin in warm environments creates additional challenges, specifically related to heat. Almost all resins will crack and deform while curing if their heat rises above the limits of the material. To avoid such issues, you need to apply the resin in thin layers and allow each to mostly cure before adding the next. I started a river table resin pour on a cold night and was able to safely apply four layers, each 1/2 inch thick. The next day, during a hot high noon, I added a fifth 1/2 inch layer and cracks appeared everywhere, penetrating down through the previous nights layers. The project was ruined and now hangs on my shop wall as a reminder to watch resin temperatures and apply resin thinly.
Make sure that you mixed the resin components in proper proportions and for long enough to achieve a homogeneous blend. If the components are not mixed thoroughly, some of the resin will cure slowly or not at all.
Not including enough hardener will definitely increase the curing time. Check the instructions to see if the proportions are by weight or by volume. 50/50 by weight can be dramatically different than 50/50 by volume.
Unrelated to your question but worth noting... working with resin in warm environments creates additional challenges, specifically related to heat. Almost all resins will crack and deform while curing if their heat rises above the limits of the material. To avoid such issues, you need to apply the resin in thin layers and allow each to mostly cure before adding the next. I started a river table resin pour on a cold night and was able to safely apply four layers, each 1/2 inch thick. The next day, during a hot high noon, I added a fifth 1/2 inch layer and cracks appeared everywhere, penetrating down through the previous nights layers. The project was ruined and now hangs on my shop wall as a reminder to watch resin temperatures and apply resin thinly.
answered Apr 19 at 14:53
Henry TaylorHenry Taylor
2,274211
2,274211
Thanks for the tips! 👍
– shripal mehta
Apr 20 at 4:57
add a comment |
Thanks for the tips! 👍
– shripal mehta
Apr 20 at 4:57
Thanks for the tips! 👍
– shripal mehta
Apr 20 at 4:57
Thanks for the tips! 👍
– shripal mehta
Apr 20 at 4:57
add a comment |
shripal mehta is a new contributor. Be nice, and check out our Code of Conduct.
shripal mehta is a new contributor. Be nice, and check out our Code of Conduct.
shripal mehta is a new contributor. Be nice, and check out our Code of Conduct.
shripal mehta is a new contributor. Be nice, and check out our Code of Conduct.
Thanks for contributing an answer to Arts & Crafts Stack Exchange!
- Please be sure to answer the question. Provide details and share your research!
But avoid …
- Asking for help, clarification, or responding to other answers.
- Making statements based on opinion; back them up with references or personal experience.
To learn more, see our tips on writing great answers.
Sign up or log in
StackExchange.ready(function () {
StackExchange.helpers.onClickDraftSave('#login-link');
});
Sign up using Google
Sign up using Facebook
Sign up using Email and Password
Post as a guest
Required, but never shown
StackExchange.ready(
function () {
StackExchange.openid.initPostLogin('.new-post-login', 'https%3a%2f%2fcrafts.stackexchange.com%2fquestions%2f6117%2fhow-to-dry-out-epoxy-resin-faster-than-usual%23new-answer', 'question_page');
}
);
Post as a guest
Required, but never shown
Sign up or log in
StackExchange.ready(function () {
StackExchange.helpers.onClickDraftSave('#login-link');
});
Sign up using Google
Sign up using Facebook
Sign up using Email and Password
Post as a guest
Required, but never shown
Sign up or log in
StackExchange.ready(function () {
StackExchange.helpers.onClickDraftSave('#login-link');
});
Sign up using Google
Sign up using Facebook
Sign up using Email and Password
Post as a guest
Required, but never shown
Sign up or log in
StackExchange.ready(function () {
StackExchange.helpers.onClickDraftSave('#login-link');
});
Sign up using Google
Sign up using Facebook
Sign up using Email and Password
Sign up using Google
Sign up using Facebook
Sign up using Email and Password
Post as a guest
Required, but never shown
Required, but never shown
Required, but never shown
Required, but never shown
Required, but never shown
Required, but never shown
Required, but never shown
Required, but never shown
Required, but never shown
BTW, a weird thing about English is that "few" and "a few" kinda mean opposite things.
– Acccumulation
Apr 19 at 14:48